Sn95Sb5
A tin-antimony alloy for joints that have to hold up in higher-temperature service.
Where it melts
| Alloy | Melting range |
|---|---|
| Sn95Sb5 | 232 to 240 °C |
Typical uses
- Higher-temperature service
- Step soldering (first joint)
- Heavy joints on large parts
Compare with
Sn42Bi58 (138 °C (eutectic))SAC305 (217 to 220 °C)SAC0307 (217 to 227 °C)Sn96.5Ag3.5 (221 °C (eutectic))All alloys in the finder